First, cohesion destruction
1. Many customers will think that the higher the temperature, the faster the glue will melt, the faster the glue, the higher the construction efficiency will be, but often too high temperature will lead to excessive heating of hot melt adhesive cohesion damage, especially when business is poor, especially large customers tend to think that this time, how much glue is added, this phenomenon may also be because the amount of glue in the glue box is too small, Excessive heating of glue results in breakage of cohesion
Two, the use process smoke
1. When the sol temperature is set too high, when the hot melt liquid level is lower than the heating plate, the heating plate will be exposed to the air for continuous heating, which will lead to the smoke of the glue box, resulting in agglomeration and carbon deposition.
Hot melt adhesive
Three, the amount of glue is not stable
1. It may be due to problems in the temperature control and heating device of the hot melt glue machine, the rubber box, hose and nozzle do not reach the specified use temperature, the operator does not add glue in time, resulting in the drop of the liquid level in the rubber box, the deposition of carbonization in the rubber box and the blockage of the filter plate and nozzle, or the setting of the spray pressure is not large enough