How To Read And Interpret HMPSA Technical Data Sheets (TDS)

Nov 08, 2026

Leave a message

How to Read and Interpret HMPSA Technical Data Sheets (TDS)

A procurement manager from a label converting company in Suzhou called me last week. He was frustrated. "I've got TDS documents from five different adhesive suppliers," he said. "They all look different. Some give me five parameters, some give me fifteen. Some use different test methods. How am I supposed to compare them?"

I understood his frustration. Technical Data Sheets (TDS) are supposed to help you make informed decisions, but when every supplier uses different formats, different test methods, and different units, they can actually make things more confusing.

The truth is, reading a TDS is a skill. It's not just about looking at numbers - it's about understanding what those numbers mean, how they were measured, and whether they're relevant to your specific application.

This guide will help you decode HMPSA technical data sheets and use them to make better adhesive selection decisions.

What Is a Technical Data Sheet (TDS)?

A Technical Data Sheet is a document provided by the adhesive manufacturer that describes the physical and performance properties of their product. It's meant to give you enough information to:

Determine if the adhesive is suitable for your application

Compare different adhesive options

Set up your application process correctly

Quality control incoming materials

A TDS is not a specification. It's a description of typical properties. Actual values may vary from batch to batch within specified tolerances. If you need guaranteed minimum or maximum values, you need a specification document, not just a TDS.

Standard Test Methods for HMPSA

Before we dive into specific parameters, you need to understand the test methods. Different test methods give different results, even for the same adhesive. Always check which test method was used.

Key Standards Organizations

FINAT (Federation of European National Associations of Tape and Self-Adhesive Product Manufacturers): The primary standards body for pressure sensitive adhesives in Europe. Their test methods are widely used globally.

PSTC (Pressure Sensitive Tape Council): The North American equivalent of FINAT. Their test methods are similar but not identical to FINAT methods.

ASTM (American Society for Testing and Materials): General testing standards that apply to many materials, including adhesives.

ISO (International Organization for Standardization): International standards that may apply to adhesive testing.

Common Test Methods

FINAT TM 1: Peel adhesion to steel at 180°

FINAT TM 2: Tack (loop tack)

FINAT TM 8: Shear resistance (static shear)

FINAT TM 9: Loop tack

FINAT TM 11: Peel adhesion to steel at 90°

FINAT TM 15: Tack (rolling ball tack)

FINAT TM 17: Resistance to elevation of temperature

FINAT TM 18: Resistance to plasticizer migration

ASTM D3121: Peel strength of pressure-sensitive adhesives

ASTM D3654: Shear adhesion of pressure-sensitive adhesives

ASTM D2979: Peel strength of pressure-sensitive adhesives

ASTM D3811: Peel adhesion of pressure-sensitive adhesives

The key point: If two suppliers report "peel adhesion" but use different test methods (e.g., FINAT TM 1 vs. ASTM D3121), the values are not directly comparable. Always check the test method.

Essential Parameters on HMPSA TDS

Let's go through the parameters you'll typically see on an HMPSA TDS, what they mean, and why they matter.

Physical Properties

Softening Point (Ring & Ball)

What it measures: The temperature at which the adhesive begins to flow

Test method: ASTM E28 or ISO 4625

Units: °C

Typical range: 70-120°C for HMPSA

Why it matters: Indicates the upper temperature limit for the adhesive. If your product will be exposed to high temperatures (e.g., in a hot car, during shipping in summer), you need a high softening point.

How to interpret: Higher softening point = better heat resistance, but potentially lower flexibility at room temperature.

Viscosity

What it measures: The resistance to flow when the adhesive is melted

Test method: ASTM D3236 or similar

Units: mPa·s (millipascal-seconds) or cP (centipoise) - these are equivalent

Test conditions: Temperature and test method must be specified (e.g., 160°C, 180°C, or 200°C)

Typical range: 2,000-10,000 mPa·s for HMPSA

Why it matters: Viscosity determines how the adhesive flows during application. Too high = poor wetting, stringing. Too low = squeeze-out, poor gap filling.

How to interpret: Always check the test temperature. Viscosity at 160°C is not the same as viscosity at 180°C. Lower viscosity = better flow and wetting, but may have more squeeze-out.

Density

What it measures: Mass per unit volume

Test method: ASTM D1475 or ISO 2811

Units: g/cm³ or kg/L

Typical range: 0.9-1.1 g/cm³ for HMPSA

Why it matters: Used to convert between weight and volume. Important for calculating coverage and cost.

How to interpret: Not a performance parameter, but useful for process calculations.

Color and Appearance

What it measures: Visual appearance of the adhesive

Test method: Visual inspection

Description: Usually described as "clear," "light yellow," "amber," etc.

Why it matters: Aesthetic requirements. Some applications require clear or light-colored adhesive.

How to interpret: Color can indicate the type of raw materials used. Clear/water-white typically indicates hydrogenated raw materials. Amber/dark may indicate non-hydrogenated materials. Color can also change with age or thermal exposure.

Performance Properties

Tack (Initial Adhesion)

What it measures: The ability to form an instant bond with minimal pressure

Test methods:

- Loop tack (FINAT TM 9, PSTC 15)

- Rolling ball tack (FINAT TM 15, PSTC 32)

- Probe tack (ASTM D2979)

Units: Newtons (N) for loop tack and probe tack; ball number or cm for rolling ball tack

Typical range: 5-30 N for loop tack

Why it matters: Tack determines how well the adhesive grabs on initial contact. High tack = instant grab. Low tack = slower bond development.

How to interpret: Higher tack is not always better. Too much tack can cause stringing, oozing, or difficulty in repositioning. Match tack to your application requirements.

Peel Adhesion

What it measures: The force required to remove the adhesive from a substrate at a specific angle

Test methods:

- 180° peel (FINAT TM 1, ASTM D3330)

- 90° peel (FINAT TM 11)

Units: N/25mm or N/inch

Test conditions: Substrate (usually stainless steel), dwell time (usually 20 minutes or 24 hours), peel speed (usually 300 mm/min or 12 in/min)

Typical range: 5-50 N/25mm on stainless steel

Why it matters: Peel adhesion indicates the strength of the bond after it has had time to develop. It's a measure of the adhesive's ability to resist removal.

How to interpret: Higher peel = stronger bond. But peel adhesion on stainless steel may not represent peel adhesion on your actual substrate. Always test on your substrate if possible.

Shear Resistance (Cohesion)

What it measures: The ability to resist sliding under a constant load

Test methods:

- Static shear (FINAT TM 8, PSTC 7)

- Dynamic shear (FINAT TM 3)

Units: Hours or minutes (time to failure under specified load)

Test conditions: Bond area (usually 25mm x 25mm or 1 in²), load (usually 1 kg or 500g), temperature (usually 23°C or 70°C)

Typical range: 100-10,000+ hours

Why it matters: Shear resistance indicates the adhesive's internal strength (cohesion) and its ability to hold a load over time. Critical for applications where the bond must support weight or resist sliding.

How to interpret: Higher shear = better holding power. But high shear often comes at the expense of tack. There's always a tradeoff between tack and shear.

Quick Stick

What it measures: The adhesion immediately after bonding, before the adhesive has had time to flow and wet the substrate

Test method: FINAT TM 16 or similar

Units: N/25mm

Why it matters: Quick stick indicates how well the adhesive grabs immediately. Important for high-speed applications where there's no dwell time.

How to interpret: Quick stick is always lower than peel adhesion after dwell. The ratio of quick stick to peel adhesion indicates how quickly the adhesive builds strength.

Application Properties

Application Temperature

What it measures: The recommended temperature range for applying the adhesive

Units: °C

Typical range: 140-180°C for HMPSA

Why it matters: Applying at the wrong temperature can cause poor wetting, stringing, or thermal degradation.

How to interpret: Always apply within the recommended range. Lower temperature = higher viscosity, poorer wetting. Higher temperature = lower viscosity, better wetting, but risk of thermal degradation.

Open Time

What it measures: The time available between adhesive application and bonding before the adhesive sets too much

Units: Seconds or minutes

Why it matters: If your process has a long delay between application and bonding, you need long open time. If the delay is short, open time is less critical.

How to interpret: Longer open time gives more flexibility in process design, but may slow production.

Set Time

What it measures: The time required for the adhesive to develop sufficient strength for handling

Units: Seconds or minutes

Why it matters: Determines how quickly you can handle the bonded assembly after joining.

How to interpret: Shorter set time = faster production, but may sacrifice ultimate bond strength.

Coat Weight

What it measures: The recommended amount of adhesive to apply per unit area

Units: g/m² or gsm (grams per square meter)

Typical range: 20-80 g/m² for HMPSA

Why it matters: Too little adhesive = weak bond. Too much adhesive = waste, squeeze-out, potential oozing.

How to interpret: Always start with the recommended coat weight and adjust based on your specific requirements.

How to Compare Different Adhesives

Comparing adhesives from different suppliers can be challenging because of different test methods, units, and formats. Here's how to do it systematically:

Step 1: Normalize the Test Methods

First, check if the test methods are the same. If not, you can't directly compare the values. You need to either:

Request data using the same test method

Use conversion factors (if available)

Test both adhesives yourself using the same method

Step 2: Normalize the Units

Convert all values to the same units. For example:

Peel adhesion: Convert everything to N/25mm or N/inch

Viscosity: Convert everything to mPa·s or cP

Temperature: Convert everything to °C

Step 3: Compare Apples to Apples

Make sure you're comparing the same test conditions:

Peel adhesion on the same substrate (stainless steel, your substrate)

Peel adhesion after the same dwell time (20 minutes, 24 hours)

Shear resistance at the same temperature and load

Viscosity at the same temperature

Step 4: Create a Comparison Table

Create a table with all the key parameters side by side. This makes it easy to see the differences.

| Parameter | Adhesive A | Adhesive B | Adhesive C |

|-----------|------------|------------|------------|

| Softening Point (°C) | 95 | 105 | 90 |

| Viscosity @ 160°C (mPa·s) | 4,500 | 6,000 | 3,500 |

| Loop Tack (N) | 18 | 12 | 22 |

| Peel Adhesion @ 20min (N/25mm) | 25 | 30 | 20 |

| Peel Adhesion @ 24h (N/25mm) | 35 | 40 | 28 |

| Shear Resistance @ 23°C (hours) | 2,000 | 5,000 | 1,000 |

| Application Temp (°C) | 150-170 | 160-180 | 140-160 |

Step 5: Weight the Parameters

Not all parameters are equally important for your application. Weight them based on your priorities:

For high-speed labeling: Quick stick and set time are critical

For heavy-duty bonding: Shear resistance is critical

For cold environments: Low-temperature flexibility is critical

For outdoor use: UV resistance and aging stability are critical

Rank each adhesive based on how well it meets your weighted priorities.

Red Flags in TDS Documents

Watch out for these warning signs:

Missing Test Methods

If the TDS doesn't specify the test method, the data is unreliable. You can't verify it or compare it to other adhesives.

Incomplete Data

If the TDS only gives you some parameters but not others, the supplier may be hiding weak points. Request complete data.

Unrealistic Values

If the values seem too good to be true, they probably are. For example, if an adhesive claims both very high tack (>25 N) and very high shear (>10,000 hours), be skeptical. There's always a tradeoff.

No Application Recommendations

If the TDS doesn't provide application temperature, coat weight, or open time recommendations, the supplier may not have tested the adhesive in real applications.

Outdated Information

Check the revision date. If the TDS is more than 2-3 years old, the formulation may have changed. Request the current version.

Vague Descriptions

If the TDS uses vague terms like "excellent tack" or "good shear resistance" without providing actual values, it's not useful. Demand specific numbers.

How to Use TDS Data for Adhesive Selection

Here's a systematic approach to using TDS data for adhesive selection:

Step 1: Define Your Requirements

Before looking at any TDS, define what you need:

Substrate materials

Application method and conditions

Performance requirements (tack, peel, shear)

Environmental conditions (temperature, humidity, UV exposure)

Regulatory requirements (food contact, biocompatibility, etc.)

Step 2: Screen Suppliers

Request TDS documents from multiple suppliers. Screen them based on:

Do they provide complete data with test methods?

Do the basic properties match your requirements?

Are the application recommendations compatible with your process?

Step 3: Shortlist Candidates

Based on the TDS data, shortlist 2-3 adhesives that best match your requirements.

Step 4: Request Samples

Request samples of the shortlisted adhesives. Test them on your actual substrates under your actual process conditions.

Step 5: Validate Performance

Don't rely solely on TDS data. Validate performance through your own testing:

Peel tests on your substrate

Shear tests under your expected loads

Environmental testing (temperature, humidity, aging)

Production trials

Step 6: Make the Decision

Based on TDS data, sample testing, and production trials, make your final decision. Consider:

Performance (does it meet your requirements?)

Process compatibility (does it work with your equipment?)

Cost (total cost, not just price per kg)

Supplier support (technical support, quality control, delivery)

Common Mistakes When Reading TDS

Mistake #1: Focusing Only on One Parameter

Don't just look at tack or peel. Consider all the parameters and how they interact. High tack often means low shear. High peel may mean poor removability.

Mistake #2: Ignoring Test Conditions

Peel adhesion on stainless steel after 20 minutes is not the same as peel adhesion on your substrate after 24 hours. Always check the test conditions.

Mistake #3: Comparing Different Test Methods

You can't compare loop tack (FINAT TM 9) with rolling ball tack (FINAT TM 15). They measure different things.

Mistake #4: Trusting TDS Data Blindly

TDS data is typical values, not guaranteed values. Always validate with your own testing.

Mistake #5: Ignoring Application Parameters

Performance data is useless if you don't apply the adhesive correctly. Pay attention to application temperature, coat weight, and open time recommendations.

Final Thoughts

Reading and interpreting HMPSA technical data sheets is a critical skill for anyone involved in adhesive selection. It allows you to make informed decisions, compare different options, and avoid costly mistakes.

Remember:

Always check the test methods and conditions

Compare apples to apples

Don't rely solely on TDS data - validate with your own testing

Consider all parameters, not just one

Use TDS data as a starting point, not the final answer

If you're struggling to interpret TDS data or select the right adhesive for your application, contact our technical team. We can help you understand the data, compare options, and select the best adhesive for your specific requirements.

---

*Boiling - block-form hot melt pressure sensitive adhesive manufacturer since 2005. ISO 9001, REACH compliant.*

*[Contact our technical team →](https://www.blhotmeltglue.com/contact-us)*

FAQs

Q: Why do different suppliers report different values for the same adhesive property?

A: Different test methods, test conditions, or units can give different values. Always check the test method and conditions. If they're different, the values are not directly comparable.

Q: Can I compare tack values from different test methods?

A: No. Loop tack, rolling ball tack, and probe tack measure different things. You can only compare values from the same test method.

Q: What's more important: high tack or high shear?

A: It depends on your application. High-speed applications need high tack. Heavy-duty applications need high shear. There's always a tradeoff between the two.

Q: Should I trust the TDS data or do my own testing?

A: Use TDS data for initial screening, but always validate with your own testing on your actual substrates and under your actual conditions.

Q: What if the TDS doesn't include a parameter I need?

A: Request the data from the supplier. If they can't provide it, that's a red flag. You may need to test it yourself.